about general matter

How about Mituya's environment management ?

We consider the environment management as a first priority. All of our factories are recognized by the external organization such as KES, EcoStage. Our certificate status

How about recognition of quality management system ?

All of our factories have ISO9001 recognition by the external organization. Addtionally, Gotanda and Hachioji factory have JIS9100 recognition for aerospace management. Our certificate status

What kind of plating Mituya can provide ?

We have provided wide range of plating and finishing solution. we are specialized in advanced functional solution at industrial plating and finishing. Please refer our platings and finishings on the below link ! Our platings and finishings

Can Mitsuya accept the small Qty prototype ?

Yes, we welcome your request from 1 piece prototype to the large volume of mass production, as discussing with you. Please do not hesitate to contact us by 'Free Quotation' or 'Contact' page on this website !

about plating metal

What is the recommended thickness of Gold plating for soldering ?

The recommended thickness of gold plating is less than 0.1 micrometer. Thicker plating causes the quality problem while soldering. Most of the case, thickness is less than 0.5 micrometer.

What kind of gold plating Mitsuya has ?

Mitsuya has provided more than 10 kinds of gold plating, depend on the product usage. Please refer our typical platings on the below link !
Our Gold platings...

How different between electro and electroless on Nickel plating ?

Electroless nickel plating has an advantage on the uniform deposit thickness, compare with electro nickel plating. The feature of electroless nickel plating are non-magnetic and low melting point. Please refer our typical platings on the below link !
Our Nickel platings...

about plating functional property

Any other low cost solution for soldering besides Gold plating ?

We propose a tin plating and a tin-copper alloy plating. And our nickel plating can also be applied, depend on the condition. Our Tin platings...

How inconstant is plating deposit thickness ?

Generally, the difference between maximum and minimum thickness is about 3 times at the same point of product. It depends on plating type and metal.

about substrate

Can we do a Gold plating on the aluminium substrate ?

Yes, we can plate, as discussing the conditions and details with customer.

Can we plate on the glass substrate ?

Yes, we can do a electroless Nickel plating on the glass substrate. The deposit thickness is 1 micrometer on the soda-lime glass, and 0.2 micrometer on the quartz glass. Plating on the glass substrate...

Can we plate on the silicon wafer substrate ?

Yes, we can do a electroless Nickel plating on mirror surface of the silicon wafer substrate with 1 micrometer deposit thickness. Plating on the silicon wafer substrate...

about industry

Do Mitsuya has any experience in the automotive industry plating ?

Yes, we have many experiences, and the majority is platings on the electric devices uesd in automotive industry. Platings by industry...

about process type

Can Mitsuya do the plating by a reel to reel process type ?

Yes, we can do the reel to reel plating at the Yonezawa factory and Kofu factory. Platings by reel to reel process...